Summary

Product identification

The RE2012-LP is a low-pressure grade reverse osmosis (RO) element designed for residential use. It is certified to NSF/ANSI 58.

General Features

  • Permeate Flow Rate: 50 GPD (189 L/day)
  • NaCl Rejection: 93% (Minimum 90%)
  • Membrane Type: Thin-Film Composite
  • Membrane Material: Polyamide (PA)
  • Element Configuration: Spiral-Wound, Tape Wrapping

Performance is based on data taken after 30 minutes of operation under the following test conditions:

  • NaCl Solution: 100 mg/L
  • Applied Pressure: 20 psig (0.14 MPa)
  • Recovery: 15%
  • Temperature: 77°F (25°C)
  • pH: 6.5–7.0

Notes:

  • Permeate flow rate for each element may vary +20% / -20%.
  • Minimum salt rejection is 90.0%.
  • All elements are vacuum leak tested using the CSM integrity test.
  • Elements can be supplied as dry or wet-type.
  • Wet-tested elements are soaked in a preservative solution (1.0% food grade SBS) and vacuum sealed.
  • For WET-TYPE storage, a 1% sodium metabisulfite solution is added as a preservative.

Dimensions

  • Model Name: RE2012-LP
  • A: 0.67 inch (17 mm)
  • B: 0.47 inch (12 mm)
  • C: 11.73 inch (298 mm)
  • D: 0.91 inch (23 mm)
  • E: 1.89 inch (48 mm)

Operating Limits

  • Max. Operating Pressure: 150 psi (1.03 MPa)
  • Max. Feed Flow Rate: 2 gpm (0.45 m³/hr)
  • Max. Operating Temperature: 113°F (45°C)
  • Operating pH Range: 2.0 – 11.0
  • Max. Turbidity: 1.0 NTU
  • Max. SDI (15 min): 3.0
  • Max. Chlorine Concentration: < 0.1 mg/L

General Handling Procedures

  • Elements in boxes must be kept dry at room temperature (7–32°C; 40–95°F) and not stored in direct sunlight.
  • Permeate from the first hour of operation should be discarded.
  • Stabilized salt rejection is generally achieved within 1–48 hours of continuous use.
  • Keep elements moist at all times after initial wetting.
  • Avoid excessive pressure and flow spikes.
  • Only use chemicals compatible with the membrane elements and components. Use of incompatible chemicals may void the element limited warranty.
  • Permeate pressure must always be equal to or less than the feed/concentrate pressure. Damage caused by permeate back pressure voids the element limited warranty.

Disclaimer: This summary is based on the provided text extract. It may not include all figures, footnotes, or the latest revisions present in the official PDF datasheet. For contractual data, always refer to the specific OEM PDF revision used on the project.

Official datasheet (PDF)

PDF datasheet

Nội dung tổng hợp từ tài liệu kỹ thuật công khai nhằm tra cứu và so sánh sơ bộ. Bản tóm tắt không thay thế bảng dữ liệu hiện hành được nhà sản xuất chứng nhận. Kiểm tra phiên bản và giới hạn thiết kế trước khi sử dụng.