Summary

Product identification

  • Product Name: SEPLITE® Monojet™SA6400 OH
  • Description: Uniform particle size, Gel Type 1, Strong base anion resin for Industrial demineralization applications.
  • Stock Code: 300487

Physical and Chemical Characteristics

  • Matrix Structure: Gel, Styrene-divinylbenzene
  • Functional group: Trimethylammonium
  • Shipping form: OH⁻
  • Physical Appearance: Light yellow to yellowish translucent spherical beads
  • Particle size: 0.73±0.05mm
  • Particle size <0.3mm: ≤0.3%
  • Particle size ≥0.85mm: ≤5.0%
  • Moisture content: 60-70%
  • Total Capacity: ≥1.0 eq/L
  • Bulk Density: 640-700 g/L
  • Density: 1050-1090 g/L
  • Whole beads count: ≥95%
  • Uniformity coefficient: ≤1.1
  • Volume change (Cl⁻ to OH⁻): Max. 25%

Applications

  • Industrial demineralization
  • Mixed bed polishing

Recommended Operating Conditions

  • Operating Temperature Max.: 70℃
  • PH Range: 0-14
  • Min. Bed depth: 800 mm
  • Pressure drop max.: 200 kPa
  • Operation linear velocity max.: 60 m/h
  • Backwash linear velocity (approx. at 20°C): 7 m/h
  • Bed expansion (approx. at 20°C, per m/h): 10 vol.%
  • Backwash Freeboard: 80-100 vol.%

Regenerant: NaOH

  • Counter current regeneration level (approx.): 50 g/L

  • Counter current regeneration concentration (approx.): 2-5 wt.%

  • Regeneration linear velocity (approx.): 5 m/h

  • Rinse linear velocity (approx.): 5 m/h

  • Rinse water requirement (slow/fast): 2-6 BV

  • Co current regeneration level (approx.): 100 g/L

  • Co current regeneration concentration (approx.): 3-5 wt.%

  • Regeneration linear velocity (approx.): 5 m/h

  • Rinse linear velocity (approx.): 5 m/h

  • Rinse water requirement (slow/fast): 10 BV

Hydraulic Characteristics

Typical values of pressure drop and bed expansion are provided in the referenced figures (Fig. 1 and Fig. 2) in the original document. Caution is advised to avoid bed loss due to over-expansion.

Precautions

  • Store in sealed containers or bags above 0°C in dry conditions, away from direct sunlight.
  • Do not mix with strong oxidizing agents, as this can cause violent reactions.
  • In case of eye contact, rinse immediately with plenty of water and consult a specialist.
  • Dispose of materials according to local regulations.
  • Dry polymers will expand upon wetting and may cause an exothermic reaction.
  • Spilled materials can be slippery.

Disclaimer This extracted information may not include all figures, footnotes, or revisions from the original OEM PDF datasheet. Contractual data must be confirmed against the specific OEM PDF revision used for the project.

Official datasheet (PDF)

Lenntech datasheet mirror

Nội dung tổng hợp từ tài liệu kỹ thuật công khai nhằm tra cứu và so sánh sơ bộ. Bản tóm tắt không thay thế bảng dữ liệu hiện hành được nhà sản xuất chứng nhận. Kiểm tra phiên bản và giới hạn thiết kế trước khi sử dụng.